Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 88.5 MPa @Strain 8.47 %, Temperature -20.0 °C |
12800 psi @Strain 8.47 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Tensile Stress | 88.1 MPa @Strain 3.70 %, Temperature -40.0 °C |
12800 psi @Strain 3.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Tensile Stress | 88.3 MPa @Strain 3.60 %, Temperature -40.0 °C |
12800 psi @Strain 3.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Tensile Stress | 88.5 MPa @Strain 8.47 %, Temperature -20.0 °C |
12800 psi @Strain 8.47 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Tensile Stress | 88.1 MPa @Strain 3.70 %, Temperature -40.0 °C |
12800 psi @Strain 3.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Tensile Stress | 88.3 MPa @Strain 3.60 %, Temperature -40.0 °C |
12800 psi @Strain 3.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Tensile Stress | 88.2 MPa @Strain 2.90 %, Temperature -40.0 °C |
12800 psi @Strain 2.90 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 88.3 MPa @Strain 3.10 %, Temperature 23.0 °C |
12800 psi @Strain 3.10 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |