Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 77.04 MPa @Strain 5.18 %, Temperature -20.0 °C |
11170 psi @Strain 5.18 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 77.04 MPa @Strain 5.18 %, Temperature -20.0 °C |
11170 psi @Strain 5.18 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Tensile Stress | 76.98 MPa @Strain 1.51 %, Temperature 40.0 °C |
11170 psi @Strain 1.51 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Tensile Stress | 76.98 MPa @Strain 1.51 %, Temperature 40.0 °C |
11170 psi @Strain 1.51 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Tensile Stress | 76.99 MPa @Strain 1.49 %, Temperature 40.0 °C |
11170 psi @Strain 1.49 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 77.02 MPa @Strain 2.67 %, Temperature 150 °C |
11170 psi @Strain 2.67 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 76.99 MPa @Strain 1.70 %, Temperature 150 °C |
11170 psi @Strain 1.70 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Tensile Stress | 77.04 MPa @Strain 0.880 %, Temperature 0.000 °C |
11170 psi @Strain 0.880 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |