Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® E 332 ABS Resin Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2.. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® F 332 ABS Resin Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther.. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
1.69 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | >= 0.900 J/cm @Temperature 23.0 °C |
>= 1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8332M (EPC40R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -20.0 °C |
1.69 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Micropol Microstat ML21 Linear medium density static dissipative polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 0.000 °C |
1.69 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 0.000 °C |
1.69 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistanceInformation provided by Cossa Po.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 0.000 °C |
1.69 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 0.000 °C |
1.69 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 1660 GFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedHigh melt flow rate, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber Characteristics: 20% glass fibre filled, excellent mechanical properties |
|||
Izod Impact, Notched | 0.900 - 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.69 - 2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
Izod Impact, Notched | 0.900 - 1.70 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.69 - 3.18 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.69 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR HI 1012 Polystyrene General purpose polystyreneHigh impact resistance, good melt flow rate, good flexibilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |