Mechanical Properties Metric English Comments
Izod Impact, Notched 1.65 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
3.09 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ISO 180/4A
Polimeri Europa Sinkral® B 432/E ABS Resin
Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet..
Izod Impact, Notched 1.65 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
3.09 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ISO 180/4A
Polimeri Europa Sinkral® C 442 ABS Resin
Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB..
Izod Impact, Notched 1.65 J/cm

@Temperature -29.0 °C
3.09 ft-lb/in

@Temperature -20.2 °F
3.2 mm (0.125 in) notch
Kraton® G1651 + PPE blend (10/90)
Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [..
Izod Impact, Notched 1.65 J/cm

@Temperature 23.0 °C
3.09 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..