Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.65 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
3.09 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Izod Impact, Notched | 1.65 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
3.09 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Izod Impact, Notched | 1.65 J/cm @Temperature -29.0 °C |
3.09 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1651 + PPE blend (10/90) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Izod Impact, Notched | 1.65 J/cm @Temperature 23.0 °C |
3.09 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |