Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature 23.0 °C |
2.10 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature 23.0 °C |
2.10 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® D1102 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.10 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature 23.0 °C |
2.10 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -18.0 °C |
2.10 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6600A Impact Copolymer Polypropylene Impact Copolymer for Extrusion and Compounding Applications (Fractional Melt Flow) Formolene® 6600A is a high impact copolymer with an excellent balance of toughness and stiffness. It is suitable f.. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -18.0 °C |
2.10 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding ap.. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -40.0 °C |
2.10 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar.. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |