Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding applications. It embodies a unique combination of polymerization technology and additive know-how that give it an excellent balance of stiffness and impact strength. Formolene 6613N offers advantages in both processing and physical properties over many polypropylenes used for pails, crates and other rugged injection molded applications. Formolene® 6613N meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength, Yield 22.8 MPa
3300 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 1.12 J/cm

@Temperature -18.0 °C
2.10 ft-lb/in

@Temperature -0.400 °F
ASTM D256
1.33 J/cm

@Temperature 0.000 °C
2.50 ft-lb/in

@Temperature 32.0 °F
ASTM D256
5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved