Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength 37.2 MPa
5400 psi
ASTM D638
Elongation at Yield 3.1 %
3.1 %
ASTM D638
Flexural Yield Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.10 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
1.49 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
2.80 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
3.04 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.70 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
Unannealed; ASTM D648
106 °C
223 °F
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Unannealed; ASTM D648
102 °C
216 °F
Annealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved