Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1102 + PP blend (10/90)

Category Polymer , Thermoplastic , Elastomer, TPE , Polypropylene (PP)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1102 + PP blend (10/90).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON D series consists of an unsaturated polymer, either butadiene or isoprene, as the rubber monomer. Information provided by the manufacturer, Kraton® Polymers.
Physical Properties Metric English Comments
Melt Flow 2.8 g/10 min
2.8 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.5 MPa
3260 psi
Tensile Strength, Yield 28.0 MPa
4060 psi
Flexural Modulus 1.40 GPa
203 ksi
Izod Impact, Notched 0.721 J/cm

@Temperature 0.000 °C
1.35 ft-lb/in

@Temperature 32.0 °F
3.2 mm (0.125 in) notch
1.12 J/cm

@Temperature 23.0 °C
2.10 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Falling Dart Impact 159 J
117 ft-lb
Falling weight impact at 23°C (73.4°F)
Users viewing this material also viewed the following: