Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.981 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene
Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection..
Izod Impact, Notched 0.981 J/cm

@Thickness 6.50 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.256 in,
Temperature 73.4 °F
ASTM D256
LG Chemical ALPHALAC SG960 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 6.50 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.256 in,
Temperature 73.4 °F
ASTM D256
LG Chemical ALPHALAC SH860 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HIPS 405AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
Izod Impact, Notched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO
Uses include electric/electronic parts.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical TR300 MABS, Flame Retardant, Transparency
Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch..
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR440 ABS, Low Emission High Heat ABS
Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR440 ABS, Low Emission High Heat ABS
Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR474F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR474F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Izod Impact, Notched >= 0.981 J/cm

@Thickness 6.40 mm,
Temperature -10.0 °C
>= 1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 14.0 °F
ASTM D256
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 0.981 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Izod Impact, Notched >= 0.981 J/cm

@Thickness 3.17 mm
>= 1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® FD-1122 PC, FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® FD-1112 PC, FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® FD-1112 PC, FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® FD-1122 PC, FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose
Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® FD-1112 PC, FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding
Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI..
Izod Impact, Notched 0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P642J Polypropylene Injection Molding
Key Characteristics:Good flowabilityExcellent stiffnessHigh impact strengthMechanical property balanceContains UV stabilizer and anti-static agentRecommended Applications:Industrial and household pr..
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm
1.84 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron KU670M ABS Heat Resistant
High rigidityInformation provided by Bhansali
Izod Impact, Notched 0.981 J/cm

@Thickness 6.40 mm
1.84 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron KU670M ABS Heat Resistant
High rigidityInformation provided by Bhansali
Izod Impact, Notched 0.981 - 1.27 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.84 - 2.39 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang.
Copyright © lookpolymers.com All Rights Reserved