Samsung Cheil Industries Infino® FD-1122 PC, FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® FD-1122 PC, FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 250 °C
35 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.7 MPa
9250 psi
50 mm/min; ASTM D638
Elongation at Break 106 %
106 %
50 mm/min; ASTM D638
Flexural Strength 93.2 MPa
13500 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.26 GPa
327 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm
1.84 ft-lb/in

@Thickness 0.250 in
ASTM D256
>= 0.981 J/cm

@Thickness 3.17 mm
>= 1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 122 °C

@Thickness 6.40 mm
252 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 143 °C
289 °F
B/50; ISO R306
Flammability, UL94 V-2

@Thickness 0.800 - 3.00 mm
V-2

@Thickness 0.0315 - 0.118 in