Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 6610A Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 6610A Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 6610A is a high impact copolymer of polypropylene designed for such injection applications as automotive compounding, lawn & garden products and appliances. It is characterized by an excellent physical property balance of stiffness and impact at room temperature and sub-ambient conditions as well as finished product dimensional stability. It contains a unique combination of stabilizers, which provide excellent processing and usage performance. Formolene® 6610A meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min

@Temperature 230 °C
10 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D2240
Tensile Strength, Yield 22.1 MPa
3200 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature -30.0 °C
1.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
0.908 J/cm

@Temperature -18.0 °C
1.70 ft-lb/in

@Temperature -0.400 °F
ASTM D256
5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648