Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.75%); ASTM-D256 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar AN001 Copolyester, Natural Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled PP homopolymer 20% chemically coupled glass fiber reinforcedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -20.0 °C |
1.50 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 1660 GFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedHigh melt flow rate, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene PP copolymer extrusion gradeFlame retardant class V2, PBDE free, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR HI 0408 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, high light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0412 Polystyrene Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber Characteristics: 20% glass fibre filled, excellent mechanical properties |
|||
Izod Impact, Notched | >= 0.800 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
>= 1.50 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |