Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.375 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.200 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
0.375 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PPE 1462  (discontinued **)
PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Izod Impact, Notched 0.200 J/cm

@Temperature -40.0 °C
0.375 ft-lb/in

@Temperature -40.0 °F
ASTM-D256
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
Practical Use; ASTM-D256
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1040 T8 V0 Flame Retardant Polypropylene
Flame retardant class V0, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene
PP homopolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene
PP homopolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 1040 TG Polypropylene, 20% Mineral Filled
PP homopolymer 20% mineral fillerGood physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 1080 TG Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent stiffness, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature 0.000 °C
0.375 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled
PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 J/cm

@Temperature -40.0 °C
0.375 ft-lb/in

@Temperature -40.0 °F
ASTM D256
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem Prisma 2910 RACO Random Polypropylene Copolymer
Prisma 2910 is a high melt flow rate random copolymer designed for injection molding applications. This product offers high impact strength at low temperatures and excellent processability. Its appl..
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem RP 141 Injection Molding Polypropylene
Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent ..
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem RP 347 Injection Molding Polypropylene
Description: RP 347 is a medium melt flow rate random copolymer designed for injection moulding. This product offers excellent transparency and gloss, very good stiffness/impact strength balance, ex..
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem RP 144 Coating Polypropylene
Description: RP 144 is a high melt flow rate random copolymer, designed for high speed coating equipments. This product features good processability, excellent gloss and weldability.Applications: Wa..
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem Symbios 4102 Polypropylene Terpolymer
Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) an..