Braskem Prisma 2910 RACO Random Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name Prisma
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Prisma 2910 RACO Random Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Prisma 2910 is a high melt flow rate random copolymer designed for injection molding applications. This product offers high impact strength at low temperatures and excellent processability. Its applications include: transparent containers for freezer storage, containers for microwave heating directly from freezer storage, and paint drums.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 33
33
ASTM-D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM-D638
Elongation at Yield 19 %
19 %
ASTM-D638
Flexural Modulus, 1% Secant 600 MPa
87000 psi
ASTM-D790
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM-D648
Vicat Softening Point 144 °C

@Load 1.02 kg
291 °F

@Load 2.25 lb
ASTM-D1525
Optical Properties Metric English Comments
Haze 28 %

@Thickness 1.00 mm
28 %

@Thickness 0.0394 in
ASTM-D1003