Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 45.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 61.0 J

@Temperature -40.0 °C
45.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM test
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade
Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells...
Impact Test 61.0 J

@Temperature -40.0 °C
45.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM test
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha..
Impact Test 61.0 J

@Temperature -40.0 °C
45.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM test
Polimeros Mexicanos Rotolene® Black Plus Polyethylene
Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and ..
Impact Test 61.0 J

@Temperature -40.0 °C
45.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM test
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a..
Impact Test 61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Impact Test 61.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
45.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Low Temperature; ARM
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The..
Impact Test 61.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
45.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Low Temperature; ARM
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th..
Impact Test 61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Colorcomp DX98735 PC
LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Impact Test >= 61.0 J

@Temperature -29.0 °C
>= 45.0 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
Key Features: excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirement..
Impact Test >= 61.0 J

@Temperature -29.0 °C
>= 45.0 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax 8623 Polypropylene Impact Copolymer
Key Features: super-high impact polypropylene copolymer resin, good stiffness, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirements in..
Impact Test 61.0 J

@Temperature 5.00 °C
45.0 ft-lb

@Temperature 41.0 °F
Montell drop weight impact strength
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer
Key Features: excellent cold impact resistance, good stiffness and impact balance, UV stabilizer, polypropylene copolymer resin, injection moldingApplications: automotive interior trim, pet carriers..
Impact Test 61.0 J

@Thickness 3.20 mm
45.0 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 3.3 m/s; ASTM D3763
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Impact Test 61.0 J

@Thickness 3.20 mm
45.0 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 3.3 m/s; ASTM D3763
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Impact Test 61.0 J
45.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Impact Test 61.0 J
45.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Impact Test 61.0 J
45.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific)
LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Impact Test 61.0 J

@Temperature 22.0 - 26.0 °C
45.0 ft-lb

@Temperature 71.6 - 78.8 °F
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved