Polymer Property : Impact Test = 34.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycolac® MG37CR ABS
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region.
Impact Test 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific)
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific)
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX05499 PC
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific)
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility
Impact Test 34.0 J
25.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Impact Test 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron CALIBREâ„¢ 7101 8 Polycarbonate, 10% Glass Reinforced
CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti..
Impact Test 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 213 ABS, General Purpose
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..