Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 28.2 - 39.5 J | 20.8 - 29.1 ft-lb | Torque Prevail |
Ritelok TL71 Stud & Bolt Threadlocker Anaerobic. High strength threadlocker for nuts, bolts, and heavy duty fasteners. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Impact Test | 28.2 - 39.5 J | 20.8 - 29.2 ft-lb | Break |
ND Industries StudGrade® 137 Permanent HT Threadlocker General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required. |
|||
Impact Test | 28.2 - 39.5 J | 20.8 - 29.2 ft-lb | Prevail |
ND Industries StudGrade® 140 Permanent Threadlocker General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m.. |
|||
Impact Test | 28.2 - 39.5 J | 20.8 - 29.2 ft-lb | Break |
ND Industries StudGrade® 146 Permanent StudGrade HD Threadlocker General DescriptionHigh strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical UsesFasteners over 1" diameter with coa.. |
|||
Impact Test | 28.2 J | 20.8 ft-lb | Instrumented Total Energy; ASTM D3763 |
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is eas.. |