Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 28.2 - 39.5 J | 20.8 - 29.1 ft-lb | Torque Prevail |
Ritelok TL71 Stud & Bolt Threadlocker Anaerobic. High strength threadlocker for nuts, bolts, and heavy duty fasteners. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Impact Test | 22.6 - 39.5 J | 16.7 - 29.1 ft-lb | Torque Prevail |
Ritelok TL90 Post Assembly Threadlocker Anaerobic. Low viscosity threadlocker for port assembly. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |