ND Industries StudGrade® 137 Permanent HT Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name StudGrade®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries StudGrade® 137 Permanent HT Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required.
Physical Properties Metric English Comments
Viscosity 6000 - 8000 cP
6000 - 8000 cP
Mechanical Properties Metric English Comments
Impact Test 22.6 - 33.9 J
16.7 - 25.0 ft-lb
Prevail
28.2 - 39.5 J
20.8 - 29.2 ft-lb
Break
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
With Primer (Fixture)
60.0 min
1.00 hour
On steel (fixture)
1440 min
24.0 hour
With Primer (Full)
1440 min
24.0 hour
On steel (Full)
Descriptive Properties Value Comments
Color Red
Gap Fill, in. 0.007