Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Chevron Phillips Chemical Company LP
Trade Name K-Resin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. Compared to KR05, XK41 offers greater polystyrene acceptance with equivalent processability. Thermoformed parts have very good clarity, very good toughness, and good stiffness.Applications: Major applications include thermoformed blister packs, cups and lids, and portion packages.Processing Recommendations:Melt Temperature: 218°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.Specification Data: When combined with at least 8% food grade polystyrene to produce articles for food contact, XK41 complies with FDA Regulation 21 CFR 177.1640.Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 7.5 g/10 min
7.5 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 18.8 MPa
2730 psi
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 251 %
251 %
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 29.5 MPa
4280 psi
Test specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 1.2075 GPa
175.14 ksi
Test specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Impact Test 28.2 J
20.8 ft-lb
Instrumented Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ASTM D648
Vicat Softening Point 69.0 °C
156 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 89.3 %
89.3 %
Processing Properties Metric English Comments
Processing Temperature <= 218 °C
<= 424 °F