Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
Network Polymers Softflex® 7000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose FormulationNordel® IP 4770P |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose FormulationNordel® IP 4770R |
|||
300% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |