Mechanical Properties Metric English Comments
300% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
Network Polymers Softflex® 7000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
300% Modulus 0.00520 GPa
0.754 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
300% Modulus 0.00520 GPa
0.754 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
300% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
300% Modulus 0.00520 GPa
0.754 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
FormulationNordel® IP 4770P
300% Modulus 0.00520 GPa
0.754 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose
FormulationNordel® IP 4770R
300% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..