Material Notes:
FormulationNordel® IP 4770R
Physical Properties Metric English Comments
Density 1.339 g/cc
0.04837 lb/in³
Mooney Viscosity 21

@Temperature 100 °C
21

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 7.00 MPa
1020 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 492 %
492 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00200 GPa
0.290 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00390 GPa
0.566 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00520 GPa
0.754 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 31.0 kN/m
177 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 75 %

@Temperature 125 °C
75 %

@Temperature 257 °F
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -15.0 °C
5.00 °F
Temperature Retraction, TR-10