Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412
Elongation at Break 490 %
490 %
ASTM D412
100% Modulus 0.0100 GPa
1.45 ksi
ASTM D412
300% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Tear Strength 125 kN/m
713 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F
Copyright © lookpolymers.com All Rights Reserved