Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | Aluminum, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | FRP Glass Polyester, Shear; ISO 4587 |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |