Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | Aluminum, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 2050 Cyanoacrylate, flexible PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 2050 Cyanoacrylate, flexible PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 735 Cyanoacrylate, toughened PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 735 Cyanoacrylate, toughened PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 6.00 - 8.00 MPa | 870 - 1160 psi | FRP Glass Polyester, Shear; ISO 4587 |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 6.00 MPa | 870 psi | steel collar and pin shear; ISO 10123 |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | PVC, Substrate Failure, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | >= 6.00 MPa | >= 870 psi | ABS, Substrate Failure, Shear; ISO 4587 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 6.00 MPa | 870 psi | steel collar and pin shear; ISO 10123 |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |