Mechanical Properties Metric English Comments
Charpy Impact >= 20.0 J
>= 14.8 ft-lb
At RT, Transverse
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours + air cooled)
Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corr..
Charpy Impact 20.0 J
14.8 ft-lb
aged 8000 hours at 760°C (1400°F)
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Charpy Impact 20.0 J
14.8 ft-lb
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 20.0 J

@Temperature -20.0 °C
14.8 ft-lb

@Temperature -4.00 °F
ThyssenKrupp XAR® EXTRA Structural Steel
This Material Specification applies to 4 to 40 mm thick plates of the wear-resistant special structural steel XAR® EXTRA. The high resistance to abrasion of XAR® EXTRA results from a special wate..
Charpy Impact 20.0 J

@Temperature -40.0 °C
14.8 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp SECURE 400 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.App..
Charpy Impact 20.0 J

@Temperature -20.0 °C
14.8 ft-lb

@Temperature -4.00 °F
ThyssenKrupp XAR® 600 Structural Steel
This Material Specification applies to 4 to 40 mm thick plates of the wear-resistant special structural steel XAR® 600. The extraordinary high resistance to abrasion of XAR® 600 results from a sp..
Charpy Impact 20.0 J
14.8 ft-lb
Hardening Temperature- 1175°C; Tempering Temperature- 540°C
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan..
Charpy Impact 20.0 J
14.8 ft-lb
Hardening Temperature- 1190°C; Tempering Temperature- 550°C
Crucible Steel CPM® Rex® 45® (HS) High Speed Steel
CPM Rex 45 is an 8% cobalt modification of M3 high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has red hardness comparable to that of M42 but offers abrasion resistance ev..
Charpy Impact 20.0 J
14.8 ft-lb
Hardening Temperature- 1165°C; Tempering Temperature- 565°C
Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS)
CPM Rex 76 is a super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It is heat treatable to HRC 68-70. Its high carbon, vanadium and cobalt contents provide abrasion resis..
Charpy Impact 20.0 J
14.8 ft-lb
V-Notch
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Charpy Impact >= 20.0 J
>= 14.8 ft-lb
At RT, Transverse
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours - air cooling)
Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi..