Material Notes:
This Material Specification applies to 4 to 40 mm thick plates of the wear-resistant special structural steel XAR® 600. The extraordinary high resistance to abrasion of XAR® 600 results from a special water quenching process.Application: The steel may be used for wear exposed structures, e.g. excavating, mining and earth-moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment and scrap presses.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 2000 MPa
290000 psi
Tensile Strength, Yield 1700 MPa
247000 psi
Elongation at Break 8.0 %
8.0 %
Charpy Impact 20.0 J

@Temperature -20.0 °C
14.8 ft-lb

@Temperature -4.00 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.5 %
<= 1.5 %
Boron, B <= 0.0050 %
<= 0.0050 %
Carbon, C <= 0.40 %
<= 0.40 %
Chromium, Cr <= 1.5 %
<= 1.5 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 1.5 %
<= 1.5 %
Niobium, Nb (Columbium, Cb) <= 0.050 %
<= 0.050 %
Other <= 0.79 %
<= 0.79 %
Carbon Equivalent
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.80 %
<= 0.80 %
Sulfur, S <= 0.010 %
<= 0.010 %