Material Notes:
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.Application: The steels may be used for purposes of ballistic protection mainly for applications like armoured limousines and valuable transporters.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 1150 MPa
167000 psi
Tensile Strength, Yield 950 MPa
138000 psi
Elongation at Break 11 %
11 %
Charpy Impact 20.0 J

@Temperature -40.0 °C
14.8 ft-lb

@Temperature -40.0 °F
Transverse
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.5 %
<= 1.5 %
Carbon, C <= 0.32 %
<= 0.32 %
Chromium, Cr <= 1.5 %
<= 1.5 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 0.70 %
<= 0.70 %
Phosphorous, P <= 0.015 %
<= 0.015 %
Silicon, Si <= 0.40 %
<= 0.40 %
Sulfur, S <= 0.0050 %
<= 0.0050 %