Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 - 36.6 GPa | 290 - 5300 ksi | Average value: 7.77 GPa Grade Count:226 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Modulus of Elasticity | 2.40 - 36.6 GPa | 348 - 5300 ksi | Average value: 14.3 GPa Grade Count:30 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |