Polymer Property : Modulus of Elasticity = 2.40 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.40 - 3.40 GPa

@Temperature 60.0 - 120 °C
348 - 493 ksi

@Temperature 140 - 248 °F
Average value: 2.87 GPa Grade Count:1
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Modulus of Elasticity 2.40 GPa
348 ksi
DIN 53457
Ineos Nova S-2200 Medium Impact Compact Polystyrene  (discontinued **)
Medium impact easy flowing polystyrene, designed for injection molding applications with short cycle times and for complicated technical parts. The product has a high stiffness and an excellent the..
Modulus of Elasticity 2.40 - 8.50 GPa
348 - 1230 ksi
Average value: 4.67 GPa Grade Count:29
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Modulus of Elasticity 2.40 GPa
348 ksi
Youngs Modulus, ASTM D638, 10%/min.
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Modulus of Elasticity 2.40 GPa
348 ksi
Youngs Modulus, ASTM D638, 10%/min.
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..
Modulus of Elasticity 2.40 GPa
348 ksi
Youngs Modulus, ASTM D638, 10%/min.
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527
Chevron Phillips Xtel® XE5300NA Polyphenylene Sulfide Alloy  (discontinued **)
Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance.Information provided by Chevron Phillips
Modulus of Elasticity 2.40 GPa
348 ksi
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Modulus of Elasticity 2.40 GPa
348 ksi
Lehmann & Voss LUVOCOM® 50/TF/15/GY77 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527
GEHR Plastics PC Polycarbonate
Polycarbonate shows a high rigidity and an extreme impact strength. Also it has a high glass transition temperature and temperature resistance. The operating temperature ranges from -60°C to appr..
Modulus of Elasticity 2.40 GPa
348 ksi
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro..
Modulus of Elasticity 2.40 GPa
348 ksi
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Modulus of Elasticity 2.40 GPa
348 ksi
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
Tisan TISAKRIL® UNR ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Modulus of Elasticity 2.40 GPa
348 ksi
Conditioned; ISO 178
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast.
Modulus of Elasticity 2.40 GPa
348 ksi
Conditioned; ISO 178
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Modulus of Elasticity 2.40 GPa
348 ksi
Conditioned; ISO 178
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead
Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast.
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
BASF Ultraform® N2520 L POM
Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-1/-2
BASF Ultramid® S3K Balance PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Modulus of Elasticity 2.40 GPa
348 ksi
1 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
Modulus of Elasticity 2.40 GPa
348 ksi
1% Secant; ASTM D638
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **)
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s..
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527-2
BASF Ultradur B 6550 PBT
Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.
Modulus of Elasticity 2.40 - 36.6 GPa
348 - 5300 ksi
Average value: 14.3 GPa Grade Count:30
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Modulus of Elasticity 2.40 - 12.3 GPa
348 - 1780 ksi
Average value: 4.64 GPa Grade Count:45
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..