Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 400.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.758 GPa
400.0 ksi
Abatron AboCast/AboCure 8109-1
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin..
Modulus of Elasticity 2.758 GPa
400.0 ksi
Abatron AboCast/AboCure 8109-11
All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process..
Modulus of Elasticity 2.758 GPa
400.0 ksi
Abatron AboCast/AboCure 8109-12
1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:..
Modulus of Elasticity 2.758 GPa
400.0 ksi
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig..
Modulus of Elasticity 2.758 GPa
400.0 ksi
Abatron AboCast/AboCure 8109-7
Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure...
Copyright © lookpolymers.com All Rights Reserved