Material Notes:
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty casting and potting.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Water Absorption 0.25 - 0.35 %
0.25 - 0.35 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
0.30 - 0.45 %
0.30 - 0.45 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 200 - 600 cP

@Temperature 120 °C
200 - 600 cP

@Temperature 248 °F
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
AboCure
<= 0.00133 bar

@Temperature 180 °C
<= 1.00 torr

@Temperature 356 °F
AboCast
0.00133 bar

@Temperature 100 °C
1.00 torr

@Temperature 212 °F
AboCure
0.00373 bar

@Temperature 120 °C
2.80 torr

@Temperature 248 °F
AboCure
0.0133 bar

@Temperature 135 °C
10.0 torr

@Temperature 275 °F
AboCure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 82.73 MPa
12000 psi
Modulus of Elasticity 2.758 GPa
400.0 ksi
Flexural Yield Strength 137.9 MPa
20000 psi
Compressive Yield Strength 117.2 MPa
17000 psi
Thermal Properties Metric English Comments
CTE, linear 60.0 - 65.0 µm/m-°C

@Temperature 20.0 °C
33.3 - 36.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.170 - 0.200 W/m-K
1.18 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C
230 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.5 - 3.7

@Frequency 1000 Hz
3.5 - 3.7

@Frequency 1000 Hz
3.5 - 3.7

@Frequency 1e+6 Hz
3.5 - 3.7

@Frequency 1e+6 Hz
3.6 - 3.9

@Frequency 50 Hz
3.6 - 3.9

@Frequency 50 Hz
Dielectric Strength 14.76 - 17.72 kV/mm

@Thickness 3.17 mm
374.9 - 450.1 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0030 - 0.0070

@Frequency 50 Hz
0.0030 - 0.0070

@Frequency 50 Hz
0.0050 - 0.010

@Frequency 1000 Hz
0.0050 - 0.010

@Frequency 1000 Hz
0.025 - 0.035

@Frequency 1e+6 Hz
0.025 - 0.035

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 130 - 140 °C
266 - 284 °F
Pot Life 90.0 min

@Temperature 120 °C
90.0 min

@Temperature 248 °F