Polymer Property : Modulus of Elasticity = 24.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.170 - 2.716 GPa

@Temperature -40.0 - 150 °C
24.7 - 393.9 ksi

@Temperature -40.0 - 302 °F
Average value: 0.783 GPa Grade Count:2
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.170 GPa
24.7 ksi
TD; ISO R527-1
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene
LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co.
Modulus of Elasticity 0.170 GPa
24.7 ksi
TD; ISO 527
Iran Petrochemical (PCC) LS0085 Low Density Polyethylene
LS0085 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: thin shrink film.Information provided..
Modulus of Elasticity 0.170 GPa
24.7 ksi
MD; ISO 527
Iran Petrochemical (PCC) LS0085 Low Density Polyethylene
LS0085 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: thin shrink film.Information provided..
Modulus of Elasticity 0.170 GPa
24.7 ksi
TD; ISO 527
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene
LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov..
Modulus of Elasticity 0.170 GPa
24.7 ksi
ISO 527-2
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat..
Modulus of Elasticity 0.170 GPa
24.7 ksi
ISO 527-2
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating
LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In..