Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.170 - 2.716 GPa @Temperature -40.0 - 150 °C |
24.7 - 393.9 ksi @Temperature -40.0 - 302 °F |
Average value: 0.783 GPa Grade Count:2 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |