Polymer Property : Modulus of Elasticity = 22.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.80 - 22.8 GPa
551 - 3300 ksi
Average value: 7.88 GPa Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Modulus of Elasticity 7.24 - 22.8 GPa
1050 - 3300 ksi
Average value: 13.4 GPa Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..