Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 7.24 GPa | 1050 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Nylon 6, 30 wt.% glass Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,.. |
|||
Modulus of Elasticity | 7.24 - 22.8 GPa | 1050 - 3300 ksi | Average value: 13.4 GPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Modulus of Elasticity | 7.24 GPa | 1050 ksi | IPC TM-650 2.4.18.3 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |