Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.51 - 19.3 GPa | 219 - 2800 ksi | Average value: 9.90 GPa Grade Count:14 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 1.51 GPa | 219 ksi | Cross; ASTM D638 |
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe.. |