Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 17.2 - 19.3 GPa | 2500 - 2800 ksi | Average value: 18.4 GPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 1.51 - 19.3 GPa | 219 - 2800 ksi | Average value: 9.90 GPa Grade Count:14 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 5.52 - 19.3 GPa | 800 - 2800 ksi | Average value: 11.7 GPa Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |