Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 2.25 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity >= 2.25 GPa
>= 326 ksi
ISO 527/ASTM D638
Quadrant EPP Monocast® MC 904P Nylon for Pile Driver Pads (ASTM Product Data Sheet)
Pile driver pads are used to prevent damage to the pile and the piling hammer. Fillers are usually made of hardwood - Azobe, for example. The disadvantage of Azobe is the 30-40% energy loss and it..
Modulus of Elasticity 2.25 - 3.50 GPa
327 - 508 ksi
Average value: 3.02 GPa Grade Count:53
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.25 GPa
326 ksi
DIN 53457
Ineos Nova S-3222 Medium Impact Compact Polystyrene  (discontinued **)
All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee..
Modulus of Elasticity 2.25 - 10.0 GPa

@Temperature 60.0 - 160 °C
326 - 1450 ksi

@Temperature 140 - 320 °F
Average value: 5.59 GPa Grade Count:7
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Modulus of Elasticity 2.25 - 15.0 GPa
326 - 2180 ksi
Average value: 6.31 GPa Grade Count:143
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..