Quadrant EPP Monocast® MC 904P Nylon for Pile Driver Pads (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Nylon
Manufacturer Quadrant Engineering Plastics Products
Trade Name Monocast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Monocast® MC 904P Nylon for Pile Driver Pads (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pile driver pads are used to prevent damage to the pile and the piling hammer. Fillers are usually made of hardwood - Azobe, for example. The disadvantage of Azobe is the 30-40% energy loss and its relatively short useful life. Azobe is also difficult to remove from the piling pad.Monocast® pile driver pads last much longer, are easy to replace, are versatile (diesel hammer, steam hammer, prefab-piling, and vibro-piling), has the right elasticity to transmit the blow without damaging the pile or piling hammer. With MC® 904P's unique properties (coefficient of restitution with computations is 0.904; deformation under load at 122°F (50°C) 2000 psi (13.8 MPa) is 0.6% per ASTM D621), less energy is lost so piles can be driven faster with greater force.Information provided by Quadrant Engineering Plastic Products (formerly DSM EPP).
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183; ASTM D792
Water Absorption 0.30 %
0.30 %
24 hour immersion; (3.2 x 50.8 mm specimen); ASTM D570/ISO 62
Water Absorption at Saturation 7.0 %
7.0 %
ISO 62 (3.2 x 50.8 mm specimen); ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M >= 70
>= 70
ISO 2039-2; ASTM D785
Hardness, Rockwell R >= 115
>= 115
ISO 2039-2; ASTM D785
Tensile Strength, Ultimate >= 65.0 MPa
>= 9430 psi
ISO 527; ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638 and ISO 527
Modulus of Elasticity >= 2.25 GPa
>= 326 ksi
ISO 527/ASTM D638
Izod Impact, Notched >= 0.320 J/cm
>= 0.599 ft-lb/in
ASTM D256A
Charpy Impact, Notched >= 0.400 J/cm²
>= 1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ISO 3146; ASTM D3418