Mechanical Properties Metric English Comments
Modulus of Elasticity 1.60 GPa
232 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Modulus of Elasticity 1.60 - 17.0 GPa
232 - 2470 ksi
Average value: 3.03 GPa Grade Count:30
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Modulus of Elasticity 1.60 - 7.30 GPa

@Temperature 60.0 - 150 °C
232 - 1060 ksi

@Temperature 140 - 302 °F
Average value: 3.70 GPa Grade Count:1
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Modulus of Elasticity 1.60 - 3.64 GPa
232 - 528 ksi
Average value: 2.37 GPa Grade Count:6
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Modulus of Elasticity 1.60 GPa
232 ksi
ISO 527
GEHR Plastics PVDF-ELS Polyvinylidene Fluoride, Electrically Conductive
Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan..
Modulus of Elasticity 1.60 GPa
232 ksi
Lehmann & Voss LUVOCOM® TPE-0900 VP Thermoplastic elastomer, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
Modulus of Elasticity 1.60 GPa
232 ksi
MD; ExxonMobil Method
ExxonMobil Label-Lyte™ 65LTR741 OPP Film
Product Description: A biaxially oriented, white opaque multi-layer polypropylene film with an expanded core, and coated with a proprietary static resistant coating on one side. The non-coated gloss..
Modulus of Elasticity 1.60 GPa
232 ksi
MD; ExxonMobil Method
ExxonMobil Label-Lyte™ 70LTR742 OPP Film
Product Description: A matte finish, coated, white, polypropylene film designed for use in demanding thermal transfer, pressure-sensitive label applications. It is also compatible with a wide range ..
Modulus of Elasticity 1.60 GPa
232 ksi
ISO 527-1
Dow BETAMATE™ 1496 V Epoxy
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle..
Modulus of Elasticity 1.60 GPa
232 ksi
MD; ExxonMobil Method
ExxonMobil Label-Lyte™ 60LH538 OPP Film
Product Description: A super white opaque polypropylene film face stock with a proprietary caviated core providing high yield and excellent opacity. The coated print surface provides exceptional ink..
Modulus of Elasticity 1.60 GPa
232 ksi
ISO 178
Addiplast Addilene J 120 M10 Polypropylene Copolymer
Low fluidity for extrusion or injectionInformation provided by Addiplast.
Modulus of Elasticity 1.60 GPa
232 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 ZP40 Nylon 66, 40% Mineral Filled
Mineral filled, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 1.60 - 2.10 GPa

@Temperature 60.0 - 120 °C
232 - 305 ksi

@Temperature 140 - 248 °F
Average value: 1.83 GPa Grade Count:1
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 1.60 - 2.20 GPa
232 - 319 ksi
Average value: 1.90 GPa Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 1.60 GPa
232 ksi
ASTM D638
ITW Plexus Plexus™ MA340 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic and composites.
Modulus of Elasticity 1.60 GPa
232 ksi
Conditioned; ISO 178
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead
Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast.
Modulus of Elasticity 1.60 GPa
232 ksi
Conditioned; ISO 178
Addiplast Addinyl PMD 20170 Nylon 66
GalvanizingInformation provided by Addiplast.
Modulus of Elasticity 1.60 - 29.0 GPa
232 - 4200 ksi
Average value: 8.94 GPa Grade Count:55
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..