Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.31 GPa | 1350 ksi | ASTM D638 |
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced
(discontinued **) Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom.. |
|||
Modulus of Elasticity | 9.30 - 25.5 GPa | 1350 - 3700 ksi | Average value: 16.3 GPa Grade Count:32 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 9.30 GPa | 1350 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Modulus of Elasticity | 9.30 GPa | 1350 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Modulus of Elasticity | 9.29 - 13.2 GPa | 1350 - 1910 ksi | Average value: 11.3 GPa Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |