Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.07 - 25.5 GPa | 300 - 3700 ksi | Average value: 10.9 GPa Grade Count:94 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 9.30 - 25.5 GPa | 1350 - 3700 ksi | Average value: 16.3 GPa Grade Count:32 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |