Modulus of Elasticity 9.29 - 13.2 GPa
1350 - 1910 ksi
Average value: 11.3 GPa Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..