Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.390 - 0.750 GPa | 56.6 - 109 ksi | Average value: 0.599 GPa Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 0.550 - 0.750 GPa | 79.8 - 109 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Modulus of Elasticity | 0.550 - 0.750 GPa | 79.8 - 109 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Modulus of Elasticity | 0.00800 - 0.750 GPa | 1.16 - 109 ksi | Average value: 0.188 GPa Grade Count:12 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |