Polymer Property : Modulus of Elasticity = 1.16 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00800 GPa
1.16 ksi
Reliance Industries METABOLIX PHO
Information provided by Reliance Industries
Modulus of Elasticity 0.00800 - 8.25 GPa
1.16 - 1200 ksi
Average value: 1.76 GPa Grade Count:224
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 0.00800 GPa
1.16 ksi
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Modulus of Elasticity 0.00800 GPa
1.16 ksi
ASTM D638
Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properti..
Modulus of Elasticity 0.00800 GPa
1.16 ksi
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Modulus of Elasticity 0.00800 - 0.750 GPa
1.16 - 109 ksi
Average value: 0.188 GPa Grade Count:12
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..