Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00800 GPa | 1.16 ksi | |
Reliance Industries METABOLIX PHO Information provided by Reliance Industries |
|||
Modulus of Elasticity | 0.00800 - 8.25 GPa | 1.16 - 1200 ksi | Average value: 1.76 GPa Grade Count:224 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 0.00800 GPa | 1.16 ksi | |
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.00800 GPa | 1.16 ksi | ASTM D638 |
Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properti.. |
|||
Modulus of Elasticity | 0.00800 GPa | 1.16 ksi | |
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.00800 - 0.750 GPa | 1.16 - 109 ksi | Average value: 0.188 GPa Grade Count:12 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |