Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Vista Metals ATP-5™ Precision Cast Aluminum Plate Used where flatness and dimensional control are critical, such as: computer & electronics, pharmaceuticals, medical testing equipment, packaging machinery, printing machinery, thermoforming tools, m.. |
|||
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Vista Metals Duramold-5™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Alcoa Excalibar® 6013-T8 Aluminum, 0.3-1.9 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Alcoa Excalibar® 6013-T8 Aluminum, 1.9-3.8 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Alcoa Excalibar® 6013-T8 Aluminum, 3.8-8.2 cm diameter Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance... |
|||
Modulus of Elasticity | 69.6 GPa | 10100 ksi | |
Alcoa Excalibar® 6013-T651 Aluminum Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. .. |
|||
Modulus of Elasticity | 69.3 GPa | 10100 ksi | |
Corning Antimicrobial Gorilla® Glass Touch Screen Glass Antimicrobial Corning® Gorilla® Glass is an antimicrobial cover glass with EPA registration as a treated article. It combines the benefits of Corning® Gorilla® Glass technology, including durabi.. |
|||
Modulus of Elasticity | 69.3 GPa | 10100 ksi | |
Corning Gorilla® Glass 3 Touch Screen Glass with NDR Gorilla® Glass 3 with Native Damage Resistance™ (NDR) is an alkali-aluminosilicate thin sheet glass that is better able to survive the real-world events that most commonly cause glass failure. Wit.. |